yes its true that mag seps work better when wet, but we have an abundant supply of ore at around 40% FE, so dont need to beneficiate so much to reach export grade 63%
What we want the 5000 gausss for is to pull out the lower grade FE from the reject material after we can recovered the high grade 63%.
Any help in the design of the EM much appreciated..
While this link isn't for a magnetic separator, it does give some information about a high strength EM. The guy that wrote it was the inventor of some thing that is in use across the world every day, Magnabend. A magnetic sheet metal bending break. https://www.aaybee.com.au/Magnabend/Building Your Own Magnabend.html
You may be able to get some information and ideas from his EM design calculations.